Reliable Supplier Inconel 718 Tubes - Superalloy InconelX-750/ UNS N07750/ AlloyX-750 Seamless Pipe, Sheet, Wire – Guojin

Short Description:


Product Detail

Product Tags

Related Video

Feedback (2)

Our target is to consolidate and improve the quality and service of existing products, meanwhile constantly develop new products to meet different customers' demands for S31254 Bar, C70600 Tubes, Alloy 617 Plate, We have been one of your largest 100% manufacturers in China. A lot of large trading businesses import products and solutions from us, so we can easily give you the most beneficial price tag with the same quality for anyone who is interested in us.
Reliable Supplier Inconel 718 Tubes - Superalloy InconelX-750/ UNS N07750/ AlloyX-750 Seamless Pipe, Sheet, Wire – Guojin Detail:

Available Products

Seamless tube, Plate, Rod, Forgings, Fasteners, Pipe Fittings

Production Standards

Product

ASTM

Bars and Forgings

B 637

Chemical Composition

%

Ni

Cr

Fe

C

Mn

Si

S

Ti

Nb+Ta

Al

Co

Cu

Min

70.0

14.0

5.0

2.25

0.70

0.40

Max

17.0

9.0

0.08

1.00

0.50

0.010

2.75

1.20

1.00

1.00

0.50

Physical Properties

Density

8.28 g/cm3

Melting

1393-1427℃

Inconel X-750 Features

Inconel X-750 alloy is mainly a nickel-based superalloy which is age-strengthened with γ[Ni3(Al, Ti, Nb)] phase. It has good corrosion resistance and oxidation resistance below 980℃, and below 800℃ It has high corrosion resistance. It has good relaxation resistance below 540°C, as well as good formability and weldability. This alloy is mainly used for the manufacture of aircraft engines that work below 800°C and require high strength. . Springs can also be used to manufacture steam turbine turbine blades and other parts, such as plates, strips, bars, forgings, rings, wires, pipes, etc.

Inconel X-750 Heat Treatment Process

The solution heat treatment system for plates, strips and pipes in the supply state is 980℃±15℃, air cooling. For the intermediate heat treatment system of materials and parts, the following processes can be selected for heat treatment.
Annealing: 955~1010℃, water cooling.
Annealing of welded parts before welding: 980℃, 1h.
Stress relief annealing of welded parts: 900℃, moisturizing for 2h.
Stress relief annealing: 885℃±15℃, 24h, air cooling.

Inconel X-750 Available Varieties and Specifications

Bars, forgings, rings, hot-rolled sheets, cold-rolled sheets, strips, tubes and wires can be supplied in various sizes.
Plates and strips are generally supplied after hot or cold rolling, annealing or solution, pickling and polishing.
Bars, forgings and rings can be supplied in the forged or hot rolled state; they can also be supplied in solution treatment after forging; bars can be supplied after solution and polished or turned, and can be supplied in cold when the order requires Pull state into place.
The wire can be supplied in the solid solution state; for the wire with a nominal diameter or thickness below 6.35mm, it can be solid solution and supplied with a cold drawing deformation of 50% to 65%; the nominal diameter or side length is greater than 6.35mm. Wire, after solution treatment, is supplied with a cold-drawing deformation of not less than 30%. For wires with a nominal diameter or side length not greater than 0.65mm, they can be supplied with a cold-drawing deformation of not less than 15% after solution treatment as required.

Inconel X-750 Application Areas

The alloy is mainly used for the manufacture of leaf springs and coil springs with high strength requirements and relaxation resistance for aero-engines operating below 800°C. It can also be used to make parts such as turbine blades. Available varieties are sheet, strip, bar, forging, ring, wire and tube.


Product detail pictures:

Reliable Supplier Inconel 718 Tubes - Superalloy InconelX-750/ UNS N07750/ AlloyX-750 Seamless Pipe, Sheet, Wire – Guojin detail pictures

Reliable Supplier Inconel 718 Tubes - Superalloy InconelX-750/ UNS N07750/ AlloyX-750 Seamless Pipe, Sheet, Wire – Guojin detail pictures

Reliable Supplier Inconel 718 Tubes - Superalloy InconelX-750/ UNS N07750/ AlloyX-750 Seamless Pipe, Sheet, Wire – Guojin detail pictures


Related Product Guide:

carry on to further improve, to guarantee merchandise high-quality in line with market and buyer standard necessities. Our organization has a top quality assurance procedure have already been established for Reliable Supplier Inconel 718 Tubes - Superalloy InconelX-750/ UNS N07750/ AlloyX-750 Seamless Pipe, Sheet, Wire – Guojin , The product will supply to all over the world, such as: Moscow, Surabaya, US, We hope we can establish long-term cooperation with all of the customers. And hope we can improve competitiveness and achieve the win-win situation together with the customers. We sincerely welcome the customers from all over the world to contact us for anything you need!
  • This is a very professional wholesaler, we always come to their company for procurement, good quality and cheap.
    5 Stars By Janet from Libya - 2017.08.18 18:38
    As a veteran of this industry, we can say that the company can be a leader in the industry, select them is right.
    5 Stars By Edwina from Frankfurt - 2018.05.22 12:13