Our business aims to operating faithfully, serving to all of our clients , and working in new technology and new machine continuously for UNS N06200 Plate, Alloy 600 Bar, Nickel Superalloy Plate, We put genuine and health as the primary responsibility. We have now a expert international trade crew which graduated from America. We are your next small business partner.
Hot New Products Nickel Superalloy Tubes - Pure Nickel UNS N02200/ N6/ Ni200 Seamless Pipe, Sheet, Bar, Strip – Guojin Detail:

Available Products

Seamless tube, Plate, Rod, Forgings, Fasteners, Pipe Fittings.

Production Standards

Product ASTM
Bar B 160
Sheets, Sheets and Strips B 162, B 906
Seamless Pipe and Fittings B 161, B 829
welded pipe B 725, B 775
Welded pipe fittings B 730, B 751
Welded connectors B 366
Forging B 564

Chemical Composition

%

Ni

Fe

C

Mn

Si

S

Cu

Min

99.5

Max

0.40

0.15

0.35

0.35

0.010

0.25

Physical Properties

Density

8.89 g/cm3

Melting

1435-1446℃

Nickel 200 Material Properties

Nickel 200 (N6) has excellent corrosion resistance, high electrical vacuum performance and electromagnetic viewing performance, and is widely used in chemical, mechanical and electronic, food and other fields. Pure nickel has excellent welding performance and processing performance, and can be processed into pipe, rod, wire, strip, and foil products. It is one of the most widely used materials in industry. It has good mechanical properties and excellent corrosion resistance in many corrosion-resistant environments, especially caustic soda corrosion.
Nickel 200 (N6) is a commercially processed pure nickel that is effective against corrosion in a variety of chemical environments. It can also be used under oxidizing conditions to passively form an oxide film, making it extremely resistant to alkali metal corrosion. Nickel 200 (N6) is limited to use below 315°C, because the increase in temperature will cause graphitization, which will seriously damage its quality. In this case, Nickel 201 is required. It has a high Curie temperature and good magnetic properties. And its thermal conductivity and electrical conductivity are higher than nickel alloys.

Nickel 200 (N6) Material Application Areas

In food processing equipment, salt refining equipment. However, the equipment and the like required to manufacture industrial sodium hydroxide under high temperature conditions above 300°C. In the field of materials, it can be used to manufacture plates, strips, round bars, and welded pipes.
Food and synthetic fibers; electrical and electronic components; aerospace and missile components; chemical storage tanks.


Product detail pictures:

Hot New Products Nickel Superalloy Tubes - Pure Nickel UNS N02200/ N6/ Ni200 Seamless Pipe, Sheet, Bar, Strip – Guojin detail pictures

Hot New Products Nickel Superalloy Tubes - Pure Nickel UNS N02200/ N6/ Ni200 Seamless Pipe, Sheet, Bar, Strip – Guojin detail pictures

Hot New Products Nickel Superalloy Tubes - Pure Nickel UNS N02200/ N6/ Ni200 Seamless Pipe, Sheet, Bar, Strip – Guojin detail pictures


Related Product Guide:

High-quality comes 1st; assistance is foremost; business enterprise is cooperation is our business enterprise philosophy which is constantly observed and pursued by our business for Hot New Products Nickel Superalloy Tubes - Pure Nickel UNS N02200/ N6/ Ni200 Seamless Pipe, Sheet, Bar, Strip – Guojin , The product will supply to all over the world, such as: Canberra, Montpellier, Nepal, Welcome to visit our company, factory and our showroom where displays various products that will meet your expectation. Meanwhile, it is convenient to visit our website, and our sales staff will try their best to provide you the best service. Please contact us if you need more information. Our aim is to help customers realize their goals. We are making great efforts to achieve this win-win situation.
  • Product quality is good, quality assurance system is complete, every link can inquire and solve the problem timely!
    5 Stars By Eartha from Guatemala - 2018.11.06 10:04
    This supplier stick to the principle of Quality first, Honesty as base, it is absolutely to be trust.
    5 Stars By Kitty from Peru - 2018.06.18 17:25