Discount Price Nickel Superalloy Bar – Pure Nickel Manufacturer UNS N0221/ N4/ Ni201 Seamless Pipe, Sheet, Bar, Strip – Guojin Detail:

Available Products

Seamless tube, Plate, Rod, Forgings, Fasteners, Pipe Fittings

Production Standards

Product

ASTM

Bar

B 160

Plate, Sheet and Strip

B 162, B 906

Seamless pipes and fittings

B 161, B 829

Welded pipe

B 725, B 775

Welded fittings

B 730, B 751

Forging

B 564

Chemical Composition

%

Ni

Fe

C

Mn

Si

S

Cu

Min

99.9

Max

0.40

0.020

0.35

0.35

0.010

0.25

Physical Properties

Density

8.89 g/cm3

Melting

1435-1446℃

Ni201 Material Properties

N02201 pure nickel is a very important metal material. It has good strength and plasticity and has been widely used in the industry. It not only forms valuable alloys with other metals, but also pure nickel has good properties. Metal properties, used alone as a corrosion-resistant structural and functional material. In fact, pure nickel used as a corrosion-resistant structural material is a carbon-containing nickel-carbon alloy.
Nickel 201 is a low carbon version of Nickel 200. Due to its lower carbon content, Nickel 201 is less susceptible to embrittlement due to intergranular precipitation of carbon or graphite if exposed to temperatures of 315 – 760°C without prolonged contact with carbonaceous materials. Therefore, nickel 200 can be replaced in an environment higher than 315 °C. However, it is cleaved by sulfur-containing compounds at 315 °C, which can be counteracted by converting it into sulfate with sodium peroxide.
Nickel 201 electronic components, evaporators, ships pure nickel shows good corrosion resistance in many acidic and alkaline environments, and is mostly used in reducing media.
The main feature of nickel 201 is the corrosion resistance of alkaline media, such as caustic potash, caustic soda, etc., so it is used in the ionic membrane caustic soda process. Nickel has good corrosion resistance in dry fluorine compared to most alloys. Nickel has also been successfully used in dry chlorine and hydrogen chloride from room temperature to 540°C. Can also be used in static solutions.
Nickel 201 has excellent mechanical properties and excellent properties, high thermal and electrical conductivity, low gas content and low vapor pressure. Nickel has good mechanical properties over a relatively wide temperature range, is easy to cold work, and has processing properties similar to low carbon steel.

Ni201 Material Application Fields

plate heat exchangers, bellows compensator expansion joints, alkali production, chemical equipment, etc.Electronic components, evaporators, boats.


Product detail pictures:

Discount Price Nickel Superalloy Bar – Pure Nickel Manufacturer UNS N0221/ N4/ Ni201 Seamless Pipe, Sheet, Bar, Strip – Guojin detail pictures

Discount Price Nickel Superalloy Bar – Pure Nickel Manufacturer UNS N0221/ N4/ Ni201 Seamless Pipe, Sheet, Bar, Strip – Guojin detail pictures

Discount Price Nickel Superalloy Bar – Pure Nickel Manufacturer UNS N0221/ N4/ Ni201 Seamless Pipe, Sheet, Bar, Strip – Guojin detail pictures


Related Product Guide:

The customer satisfaction is our primary goal. We uphold a consistent level of professionalism, quality, credibility and service for Discount Price Nickel Superalloy Bar – Pure Nickel Manufacturer UNS N0221/ N4/ Ni201 Seamless Pipe, Sheet, Bar, Strip – Guojin , The product will supply to all over the world, such as: Bangladesh, Suriname, Florida, We believe with our consistently excellent service you can get the best performance and cost least goods from us for a long term . We commit to provide better services and create more value to all our customers. Hope we can create a better future together.
  • It is not easy to find such a professional and responsible provider in today's time. Hope that we can maintain long-term cooperation.
    5 Stars By Florence from Frankfurt - 2018.12.11 11:26
    Perfect services, quality products and competitive prices, we have work many times, every time is delighted, wish continue to maintain!
    5 Stars By Mandy from Puerto Rico - 2018.11.06 10:04